Aluminum Wire

Aluminum Wire

Aluminum and aluminum alloy welding wires can be divided into aluminum-magnesium, aluminum-silicon and pure aluminum welding wires. Characterized by excellent anti-corrosion capacity and relatively high joint strength, aluminum-magnesium welding wires can be applied to fields such as ship heavy industry, cryogenic vessels, power plants, railway construction, etc.; with excellent fluidity and permeability, silicon-containing aluminum alloy is suitable for the connection of hard aluminum, castings and forged alloys.
It can be used for industries such as shipbuilding, automobile manufacturing, food, repair and maintenance, etc.; welds produced by pure aluminum consumables are ductile and can be stretched or hammered without breaking. So pure aluminum consumables can be applied to industries such as chemicals, food, electronics, repair and maintenance.

Specifications

Aluminum Wire
NO.1234567
Trade nameJS.ER4043JS.ER4047JS.ER5356JS.ER5183JS.ER5087JS.ER1070JS.ER1100
Standard/GradeGB/T 10858 AWS A5.10 ER4043GB/T 10858 AWS A5.10 ER4043GB/T 10858 AWS A5.10 ER4043GB/T 10858 AWS A5.10 ER4043GB/T 10858 AWS A5.10 ER4043GB/T 10858 AWS A5.10 ER4043GB/T 10858 AWS A5.10 ER4043
Example of chemical composition of deposited metal (wt%)Si5.0012.000.0450.1200.0500.1200.350
Fe0.1300.1100.1400.0900.1300.1200.350
Cu0.0260.0600.0220.0200.0200.0020.080
Mn0.0020.0300.1300.7500.7600.0020.021
Mg0.0020.0305.0005.0004.8000.0200.021
Cr––0.1100.1200.080––
Zn0.0040.0400.0200.0300.0200.0020.021
Ti0.026–0.1000.0200.0210.002–
Zr––––0.130––
Al–––––99.7099.50
Example of mechanical properties of deposited metalMelting point℃630580635640630650650
Tensile strength MPa1751802752803009090
Brinell hardness number45506565651515
Impact value J (℃)–––––––
Diameter (φmm)MIG  Diameter:  0.8/0.9/1.0/1.2/1.6   TIG  Diameter:  1.6/2.0/2.4/3.2/4.0
PackagingMIG  welding  wires  are  7kg  or  2kg  plastic  plate  packaging.  TIG  welding wires  are  5kg  plastic  pipe  and  10kg  carton  packaging.