The Complete Guide to TIG Welding Aluminium Gas

When selecting gas for TIG welding aluminium, understanding the right type and proper application is crucial for achieving quality welds. This comprehensive guide will help you master TIG welding aluminium gas selection and usage.

Choosing the Right Shielding Gas

Pure Argon:
  • Suitable for aluminium less than 12 mm thick
  • Provides excellent arc stability and cosmetic welds
  • Ideal for beginners and general applications
  • Note: This gas facilitates cathodic cleaning in AC welding, essential for removing aluminium oxides
Argon-Helium Mixtures:
  • For aluminium thicker than 12 mm
  • The addition of helium makes the arc hotter, improving heat transfer and penetration
  • Common ratios: 75% argon / 25% helium (moderate penetration) or 50% argon / 50% helium (for maximum penetration)

Gas Flow and Cup Size Settings

The correct gas flow rate ensures proper shielding without wasting gas. This depends on your cup size (the nozzle at the end of your torch):
  • Size 5 cup: 5-6 litres/minute. This size is ideal because the arc tends to wander in AC current but stays within the argon shield, providing better control.
  • Size 7 or 8 cup: 7-9 litres/minute. Use these larger cups for thicker aluminum or wider joints.
  • For outdoor welding or in drafty conditions, increase the flow slightly (by 1-2 litres/min).
  • Using a gas lens can also improve gas coverage and reduce turbulence, especially for larger cups.

Recommended Equipment

Getting the right tools simplifies the process: Tungsten Electrode:
  • Use a 2% lanthanated tungsten electrode
  • It delivers a stable arc and works well with alternating current (AC)
  • For most applications, choose a 3.2 mm diameter electrode
  • Note: It’s important not to contaminate your tungsten electrode
Welding Torch:
  • A size 5-8 ceramic cup is standard for beginners.
  • Start with a smaller cup (Size 5) as it provides better arc control for aluminum
  • Larger cups may be needed for thicker aluminum or wide joints
Power Source:
  • Use a TIG welder with AC capabilities to remove aluminum oxide through cathodic cleaning action

Step-by-Step Guide to TIG Welding Aluminum

Prepare Your Metal:
  • Grind the oxide layer off even on new-looking aluminum
  • Clean with stainless steel brush in one direction to remove contaminants
  • Ensure both the base metal and filler rod are free from oil or contaminants
  • Aluminum can have dirt and oils within the metal itself, so cleaning is crucial even if it looks new
Set Up Your Torch:
  • Select the correct tungsten electrode, gas flow rate, and cup size
  • Use a size 5 cup if possible for better control
  • Confirm proper gas is flowing (you should feel a gentle breeze at the nozzle).
Start Welding:
  • Use a torch angle of about 15-20 degrees
  • Start slower until the puddle forms properly; Aluminum has a small range where it flows and welds
  • Let the puddle warm up before moving
  • Maintain a short arc length (2-3 mm from the metal surface)
  • Add filler rod steadily into the molten weld pool as you move along
  • Keep consistent movement
Inspect Your Weld:
  • A good weld will have a shiny, smooth appearance.
  • If you notice porosity, black spots, or uneven beads:
    • Double-check gas flow, cleanliness, and your technique
    • The white, smokey stuff can indicate tungsten contamination

Common Problems and Solutions

Many issues in TIG welding aluminium gas can be traced back to improper gas selection or flow rates. Understanding these problems helps achieve better results: Porosity (Bubbles or Holes):
  • Cause: Low gas flow, contamination, or drafts
  • Solution: Increase gas flow, clean the metal properly, and weld in a sheltered area
Black Spots or Soot:
  • Cause: Incorrect shielding gas or too low flow rate, or improper cleaning
  • Solution: Use pure argon and adjust flow to recommended levels, clean your metal properly
Weak Welds or Cracks:
  • Cause: Insufficient heat or improper filler material
  • Solution: Use helium-argon mixes for thicker aluminum and ensure the arc penetrates properly
Wide Area of Softened Material:
  • Cause: Excessive heat
  • Solution: Adjust amperage or increase travel speed to prevent the heat from spreading too far

Frequently Asked Questions (FAQ)

Q1: What is the best shielding gas for TIG welding aluminium?

A: Pure argon is best for beginners and thin aluminium (less than 12 mm). For thicker sections, argon-helium mixtures provide better penetration.
A: No, CO₂ or argon/CO₂ mixtures are not suitable for TIG welding aluminium. These gases can contaminate the weld and ruin the tungsten electrode.
A: Use a 2% lanthanated tungsten electrode with a balled tip for AC welding.