1. Introduction to TIG Welding
TIG (Tungsten Inert Gas) welding, also known as GTAW (Gas Tungsten Arc Welding), is a precise welding method that uses a non-consumable tungsten electrode to produce the weld.
Key Benefits:
- High-quality, clean welds
- Suitable for thin materials and delicate work
- Versatile across many metals including steel, aluminum, and titanium
2.Safety First: Protecting Yourself and Your Workspace

- Put on your auto-darkening welding helmet (shade 10-13)
- Wear thick leather gloves that allow finger dexterity
- Ensure all skin is covered with flame-resistant clothing
- Set up in a well-ventilated area
- Clear your workspace of flammable materials
- Locate your fire extinguisher
3. Prepare Your Metal: The Foundation of Good Welds
Different metals require different preparation: For Steel/Stainless Steel:- Use a grinder or wire brush to remove all paint, rust, and scale
- Wipe with acetone to remove oils (avoid touching cleaned area)
- Use a stainless steel brush dedicated ONLY to aluminum
- Brush in ONE direction to break up the oxide layer
- Clean until bright and shiny
- Wipe with acetone for a final clean
4. Machine Setup: Getting Connected

Proper setup is crucial for successful TIG welding. While specific steps may vary slightly between machines, here’s a general guide. Always refer to your welder’s manual for precise instructions.
- Ensure the welder is unplugged before setup.
- Connect the work clamp to your workpiece (or welding table)
- Insert into the positive (+) socket
- Tighten connection securely
- Setup your TIG torch:
- Choose the right tungsten
- For most applications, start with 2% Lanthanated (blue) tungsten. It’s versatile and works well for steel, stainless steel, and aluminum.
- Prepare the Tungsten
- For DC welding: Grind tungsten to a sharp point with a slight flat tip. This focuses the arc for precision.
- For AC welding: Leave a slight ball on the tungsten tip, which forms naturally during welding.
- Install tungsten with 3-5mm stick-out from the gas cup
- Connect the TIG torch
- Insert the power cable into the negative (-) socket
- Attach the gas line to the machine’s gas outlet
- Choose the right tungsten
- Setup the gas:
- Select your gas: 100% argon is suitable for most TIG applications
- Connect gas supply:
- Attach regulator to argon cylinder
- Connect gas hose from regulator to machine’s gas inlet
- Set flow rate: 8-10 L/min is standard for most applications
- Plug in the machine and turn on the gas at the cylinder.
- Set initial machine parameters:
- Choose AC or DC mode based on material (AC for aluminum, DC for steel)
- Set amperage according to material thickness
- Adjust gas flow rate
Check out this 1-minute JASIC TIG welding machine setup guide.

5. Dialing In Your Settings
Use this table as a starting point, but always test on scrap material first:
| Material | Mode | Filler Rod Type | Thickness (mm) | Amperage (A) | Tungsten Size (mm) |
| Carbon Steel | DC | ER70S-2 | 1.6 | 10-80 | 1.6 |
| 3.2 | 90-150 | 2.4 | |||
| 4.8 | 140-200 | 2.4 | |||
| Stainless Steel | DC | ER308L | 1.6 | 50-90 | 1.6 |
| 3.2 | 85-140 | 2.4 | |||
| 4.8 | 125-200 | 2.4 | |||
| Aluminum | AC | ER4043 | 1.6 | 55-75 | 1.6 |
| 3.2 | 90-140 | 2.4 | |||
| 4.8 | 125-180 | 2.4 |
Key Machine Settings:
- Set your polarity (DC- for carbon steel and stainless steel, AC for aluminum).
- Adjust amperage based on material thickness (start at the lower range to avoid burning through thin materials).
6. Welding Technique: The Four-Step Process
Step 1: Test Arc and Puddle
- Practice on scrap material
- Observe how changes in arc length affect puddle size
- Try some “dry runs” without filler to practice torch movement
Step 2: Start Your Weld

- Position yourself comfortably with something to steady your hands
- Hold torch at 15-20° angle to the workpiece
- For TIG welding, always use a “push” angle (75° in direction of travel)
- Adjust work angle based on joint type:
- T-joint/Fillet: 45° work angle
- Butt joint: 90° work angle
- Lap joint: 60-70° work angle
- Keep tungsten about 3mm from the metal
- Slowly create a small puddle before moving



7. Troubleshooting Common Issues
| Problem | Likely Cause | Quick Fix |
| Porous, sooty welds | Insufficient gas coverage | Increase flow rate, check for drafts |
| Tungsten contamination | Dipping electrode in puddle | Maintain proper arc length, regrind tungsten |
| Lack of fusion | Travel speed too fast or low amperage | Slow down, increase amperage slightly |
| Burn-through on thin material | Too much heat | Reduce amperage, increase travel speed |
Pro Tip: If you’re consistently having issues, step back and re-check your basics: cleanliness, gas flow, and machine settings.
8. Post-Weld Care and Maintenance
- Allow welds to cool naturally (don’t quench with water)
- Brush welds to remove any oxide layer (stainless steel brush for stainless)
- Inspect your welds for uniformity and potential defects
- Clean your tungsten electrode if contaminated
- Turn off the gas at the cylinder when finished
Equipment Care:
- Store tungsten electrodes in a clean, dry place
- Regularly check all cable connections for tightness
- Keep your welding table clean and free of debris
Remember, TIG welding is a skill that improves with time and patience. Focus on developing smooth, consistent movements, and don’t get discouraged if your first welds aren’t perfect. Every experienced welder started as a beginner!
For more resources, check out our other articles.
Frequently Asked Questions (FAQ)
Q: How do I choose the amperage for TIG welding?
A: Follow this process:
- Refer to our settings table(Section 5) for specific ranges
- Test on scrap material:
- Start at the lower end of the range
- Gradually increase until you achieve proper penetration
Q: How far should my tungsten stick out?
- Standard cups: 3-5mm stick-out
- Key considerations:
- Longer stick-out = Better visibility but weaker gas coverage
- Shorter stick-out = More gas protection but limited access